Are Crackling Microstars used as a core for stars an effect worth pursuing? I don’t seem to be able find a video of this effect but I’m not sure what I’m looking for. I’m thinking of a blue star from "Chemistry of the Elements" which is formulated as follows
Ammonium perchlorate 48
Hexamine 14
Copper oxychloride 12
Copper sulfate 6
Gum arabic 1
Dextrin 6
With a Crackling core of by “Larry Stevens”
Lead Tetraoxide 10
Copper (II) Oxide 7
Magnalium, granular -200 mesh 4
Potassium Nitrate 1.5
Sulfur 1
Bound together with N.C
Further questions are…
Will the cores need priming?
Will the stars need priming?
Will there be any incompatibility problems?
Any input would be much appreciated.
Regards,
Vic.
#2
Posted 12 October 2008 - 10:33 PM
#3
Posted 12 October 2008 - 10:59 PM
Yes, they are worth pursuing, an excellent effect, especially if you add some fine-ish flake titanium into the crackle mix, anyone who has seen the Yung Feng "chrysanthemum with crackling balls" shells will concur I;m sure. However you have a couple of chemical incompatibilities between your 2 mixes: 1) AP + KNO3 = ammonium nitrate = hygroscopic = mush. 2) AP + magnalium (unless dichromate passivated) = magnesium perchlorate = hygroscopic + heat generation, not good.
Thankyou for your reply, if my cores are bound with NC and the stars with dextrin does this limit the crossover incompatablity
#4
Posted 13 October 2008 - 05:35 PM
Edited by pyrotrev, 13 October 2008 - 05:37 PM.
#5
Posted 14 October 2008 - 06:15 PM
Vic
#6
Posted 15 October 2008 - 04:17 PM
#7
Posted 15 October 2008 - 08:37 PM
Vic
#8
Posted 17 October 2008 - 12:05 PM
I believe Shimizu quotes one with just fine aluminium flakein one of his papers, but I don't have the mix. Otherwise it's dichromate passivating the magnalium or using a a KClO4 colour comp.I don’t know of a crackle mix that doesn’t use magnalium. I could go the way of a flash core such as Shimizu brilliant core as this maybe the way to go, though this has own incompatibilities resulting in the need of Boric Acid
Vic
#9
Posted 17 October 2008 - 09:07 PM
Vic
#10
Posted 17 October 2008 - 09:37 PM
I don’t think I will go the Potassium Dichromate way as it seems it’s pretty nasty stuff with a whole load of safety issues involved. I don’t have a chemistry background though I’m learning so I put Dichromate high on my one to ten risk assessment. But how about linseed oil?
Vic
I agree dichromate should be high up on the nasties list, however with the proper PPE one should not be scared of it there are plenty of other nasties that we use. It is certainly far easier to use than linseed oil. It has solved a few problems for me in some of my experiments.
#11
Posted 17 October 2008 - 10:06 PM
I agree dichromate should be high up on the nasties list, however with the proper PPE one should not be scared of it there are plenty of other nasties that we use. It is certainly far easier to use than linseed oil. It has solved a few problems for me in some of my experiments.
As I am using magnalium which has been bought already in the form of magnalium, can I treat it as a whole with the Dichromate in order to “get at” the magnesium?
Thanks for all the help so far,
Vic.
#12
Posted 17 October 2008 - 10:17 PM
As I am using magnalium which has been bought already in the form of magnalium, can I treat it as a whole with the Dichromate in order to “get at” the magnesium?
Thanks for all the help so far,
Vic.
Yep the only way to do it is to passivate the the whole lot. The idea is to create a passive oxide layer on the surface of the metal, all you are trying to do is create a layer which is not prone to attack.
Are you a member of passfire? If so just look at the article on dichromate treating magnesium and do the same with your magnalium. If you are not a member I can PM you a procedure if you want.
D
#13
Posted 18 October 2008 - 10:48 AM
Thanks Vic
#14
Posted 18 October 2008 - 07:35 PM
I would be interested in the procedure, but I'm not a member there. Could you be persuaded to show it here?Are you a member of passfire? If so just look at the article on dichromate treating magnesium and do the same with your magnalium.
All I have done to treat my magnesium is soak with cold 10% W/W potassium dichromate in deionised water for two hours, drain then air dry. I don't recall exactly where this procedure came from, possibly rec.pyro.
#15
Posted 19 October 2008 - 12:50 AM
BTW, if you use a coarser MgAl, you will get less crackles per cube. 60 mesh is usually what I use, and I get 1 crack per unit. I don't think it will cause a problem. They all will go off at slightly different times, so it will probably just be a little more sustained effect.
I've never seen dragon eggs using only Al, but I have seen a few with a mix. I have no idea what purpose the Al serves though.